Custom Lighting Extrusion Tooling

Profile design, tooling design, mould machining, trial extrusion and profile adjustment – the stage that decides whether a section runs clean in production.

Tooling is where a profile succeeds or fails

Two sections can look identical on a drawing and behave completely differently on the line. Material flows to the thickest part of a section, thin walls cool faster than thick ones, and internal corners concentrate stress. A die that ignores these produces a profile that bows, twists or holds no tolerance – however good the drawing was.

Because we design and machine tooling ourselves, trial results feed straight back into die adjustments instead of into a round of emails with a third party.

Tooling sequence

  1. Profile design – the section is finalised for extrusion, not just for drawing
  2. Tooling design – die geometry designed around material flow and cooling
  3. Mould machining – die and calibration tooling machined in-house
  4. Trial extrusion – first run to see how the section actually behaves
  5. Profile adjustment – die refined until section, tolerance and surface are right
  6. Production tooling – released for volume runs once samples are approved
Adjustment is normal, not a failure. Expect at least one trial-and-adjust cycle on a new section; complex optical profiles can need more. We build that into the schedule rather than treating it as a surprise.

What we work to

Tooling and die - capability envelope
Critical die dimensions±0.1 mm on the dimensions that carry the fit
Section widthup to 400 mm across the profile
Die typessingle-material and co-extrusion dies
MaterialsPC and PMMA, including UV-capped co-extrusion
Sample to mass productionaround 6 weeks, tooling included
Die maintenanceplanned by run length - optical geometry is monitored
Minimum orderfrom 500 pcs per profile
Production lines20+ extrusion and co-extrusion lines
Tooling ownershipbuilt for your section and maintained for the life of the part

The die is the product. Everything the profile does – fit, optics, consistency over a long run – is a consequence of how the die was cut and how it is maintained.

What the die decides

Tooling is where a custom profile is really made. The drawing sets intent, but the die sets the result: how evenly the wall cools, whether the section holds its shape, and whether fine optical geometry survives the first kilometre or the fiftieth.

The section review before the die is cut is the highest-value hour in the whole job. Wall thickness that varies across a section cools unevenly and pulls the profile out of shape; sharp internal corners concentrate stress and make the die fragile; tolerance called out on dimensions that carry no function forces hand finishing and a slower line. All three are cheap to fix at this stage and expensive afterwards.

Co-extrusion dies are the demanding end. Two melt streams have to meet in the die and stay bonded through the cooling and haul-off, which makes the first-off check longer and the die more sensitive to temperature and speed. The payoff is material only where it does work – an optical face, a UV cap, or an opaque body – in one pass.

Optical geometry is the first thing any die loses. Prisms and lenticular detail soften as the die wears, which is why optical performance is held by maintenance intervals and measurement rather than by a tolerance callout. Tell us the run length you expect and the interval gets planned with it.

What to put on the drawing

  • Section at 1:1 with wall thickness dimensioned separately
  • Which dimensions carry the fit – mark them and drop the rest
  • Single material or co-extrusion, and where each material goes
  • Optical geometry in the section, if any
  • Expected annual volume – it sets how the die is built
  • Target date and first-off approval route

Where tooling goes wrong

Four problems account for most of the tooling that has to be reworked, and all four are visible on the drawing before any steel is cut.

Uneven wall thickness

It cools unevenly and the section pulls out of shape. The most common cause of a first-off that does not fit.

Blanket tolerance across the section

Forces hand finishing and a slower line for dimensions that carry no function. Mark the ones that matter.

Optical geometry assumed to be permanent

Prisms soften as a die wears. Long runs need a maintenance interval planned with the tooling, not after the beam starts drifting.

Co-extrusion treated as a material swap

Two melt streams have to stay bonded through cooling and haul-off. It changes the die, the first-off check and the process window.

Tooling is the one cost that cannot be corrected later. The section review before it is cut is what keeps the six-week schedule honest.

What tooling has to solve

  • Uniform wall thickness so the section cools evenly and holds shape
  • Material flow balanced so thin sections fill and thick sections do not sag
  • Calibration and cooling matched to the section, not to a generic setting
  • Optical surfaces - prism and lens geometry - held along the full length
  • Straightness and twist controlled for long linear runs
  • Surface finish free of flow lines, die marks and chill marks

Frequently Asked Questions

Tooling made for your profile is your project tooling. We confirm ownership terms in the quotation so there is no ambiguity later.
Yes – adjustment is a normal part of development. Trial extrusion shows where the section needs correction, and the die is refined before production release.
It depends on section complexity. We quote tooling lead time with the quotation rather than giving a generic figure.
If you have existing tooling, we can assess it and advise whether it can be run or modified on our lines.
It is built for your section and maintained for the life of the part. It is not reused for another customer profile.
On the dimensions that carry the fit, yes. Across the whole section it is usually unnecessary and it makes both the die and the line slower.
It depends on the material, the abrasiveness of the compound and the run length. Optical geometry is monitored and maintained on an interval rather than left to wear.

Send us your drawing or sample

Our engineers review geometry, material and tooling feasibility and come back with a profile proposal and quotation.